Bitumen 60-70 80-100
No. Characteristics Value (Typical) Method
Grade
60/70
Grade
80/100
1.

Specific Gravity @ 25/25 deg C

1.01/1.06 1.01/1.05 D-70
2.

Penetration @ 25 deg C

60/70 80/100 D-5
3.

Softening Point deg C

49/56 45/52 D-36
4.

Ductility @ 25 deg C

100 min 100 min D-113
5.

Loss on Heating (wt)%

100 min 0.5 max D-6
6.

Drop in Penetration after heating%

20 max 20 max D-6 & D-5
7.

Flash Point deg C

250 min 225 min D-92
8.

Solubility in CS2 (WT%)

99.5 min 99.5 min D-4
9.

Spot test

Negative Negative *A.A.S.H.O.T 102
Crude Oil
CRUDE OIL From SAUDI
Test Method Result
Appearance Visual Brownish Black Homogeneous oil
Ash Content % wt. ASTM D482 < 0.1%
Calorific Value ( Gross ) Kcal / Kg ASTM D240 10381
Water content % vol ASTM D95 1 to 2 %
Distilation ASTM D86  
IBP °C 76.0
10% vol recovered at °C 154.0
20% vol recovered at °C 192.0
50% vol recovered at °C 302.0
60% vol recovered at °C 338.0
Cracked at °C 345.0
volume recoverd at 345°C % vol 63%
Density at 15 °C,Kg/l ASTM D4052 0.8734
Flash Point (COC) °C ASTM D93 < 25
Sulphur content % wt ASTM D4294 0.85
Rubber Process Oil (RPO)
No.

Characteristics

Value (Typical)
1.

Kinematic Viscosity at 100 deg C

35
2.

Flash Point deg C

246
3.

Pour Point deg C

15
4.

Density @ 15 deg C

1.02 kg/ cu.m.
5.

Specific Gravity @ 15 deg C

995
6.

Aniline Point deg C

45
7.

Sulphur Content

4%
8.

Ash Content deg C

02/0
9.

VGC

925/0
Fuel Oil / Furnance Oil

Category

Furnace Oil
No.

Characteristics

Value

Test Method

1.

Specific Gravity @ 60 deg F

0.8671

 ASTM D 1298

2.

Viscosity cSt @ 50 deg C

5.94

ASTM D 445

3.

Flash Point PMCC deg C

<25

ASTM D 92

4.

Pour Point deg C

<-22

ASTM D 97

5.

Water by distillation, Vol %

Trace

ASTM D 95

6.

Gross Heat of combustion, K Cal/Kg

10403

ASTM D240

7.

Sulphur wt%

1.83

ASTM D 129

8.

Total Sediment

0.71

ASTM D 4870

9.

Ash Content, wt %

0.086

ASTM D 482

10.

Sodium - ppm

Nil

AES-MOA

11.

Vanadium - ppm

11

AES-MOA

12.

Aluminium – ppm

3.5

AES-MOA

13.

Silica - ppm

Nil

AES-MOA

14.

Nickel - ppm

4

AES-MOA

D2
Test Guarantee Method
Ash, wt% Max 0.01 ASTM D-482
Carbon Residue, 10%
Bottoms. Wt%
Max 0.35 ASTM D-524
Cold Flow Properties, °C (°F)
Either
Cloud Point
Winter : Nov. – Feb.
Intermediate : Oct. & March
Summer : Apr. – Sep.
Or
Cold Filter Plugging Point
Winter : Nov. – Feb.
Intermediate : Oct. & March
Summer : Apr. – Sep.
And
Difference Between Cloud point and CFPP
(Note A)
Max +2 (36)
Max +6 (43)
Max +12 (54)
 
Max +2 (36)
Max +6 (43)
Max +12 (54)
Max 10 (18)
(Note B)
ASTM D-2500
Or ISO 3015 Or
ASTM D-5771, D-5772, D-5773


 

IP-309  
Color Max 3.0 ASTM D-1500
Corrosion Cu Strip, 3 Hrs @ 50°C (122°F) Max #3 ASTM D-130
Distillation (%Recovered)
85% Point  °C (°F)
End Point
Max 350 (662)
To be Reported
ASTM D-86 or D-2887*
(* in conjunction with
ASTM D -86 correlation)
Sulfur wt% Max 1.0
(Note B)
ASTM D-4294, ASTM D-129,
ASTM D-1266 (Note C),
ASTM D-1552
Flash, P.M. Closed, °C (°F) Min 55(131) ASTM D-93, ASTM D-93 Auto Flash Tester
Gravity, °API,
Specific, 60 °F/60 °F
To be Reported ASTM D-287 or ASTM D -4052

Viscosity :
CST @ 40°C or
SUS @ 104 °F

(Min-Max)
1.9 - 4.1
32.6 – 40.1
ASTM D- 445, ASTM D- 88
Or
ASTM D- 7042-04
Water & Sediment by
Centrifuge Vol%
Max 0.05 ASTM D- 2709
Scrap - HMS1 & HMS2
 
 
TMT BAR IS - 1786 -1985 FE - 415.
8MM/10MM/12MM
 